Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 163 °C | 325 °F | Open Cup |
Dow Corning XIAMETER® PMCPPMX-0225 Silicone Fluid Is chemically equivalent to DOW CORNING® 225 FLUID. This product is a clear, low viscosity polydimethylsiloxane polymer with unique alcohol solubility for use in antiperspirants / deodorant applica.. |
|||
Flash Point | 163 °C | 325 °F | ASTM D92 |
ChevronTexaco Elite-Cut® NH Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Flash Point | 163 °C | 325 °F | ASTM D92 |
ChevronTexaco Elite-Cut® NL Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Flash Point | >= 163 °C | >= 325 °F | |
Dow SPECTRIM™ 35B-S Polyol SPECTRIM™ 35B-S reaction moldable polymer is one component (SPECTRIM™ 35A is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology dev.. |
|||
Flash Point | >= 163 °C | >= 325 °F | |
Dow SPECTRIM™ 50B-S Polyol SPECTRIM™ 50B-S reaction moldable polymer is one component (SPECTRIM™ 35B-S is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology d.. |
|||
Flash Point | >= 163 °C | >= 325 °F | Open Cup |
Dow Corning XIAMETER® PMCPPMX-200 10CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 10CS. 100% active, 10 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |