Material Notes:
Is chemically equivalent to DOW CORNING® 225 FLUID. This product is a clear, low viscosity polydimethylsiloxane polymer with unique alcohol solubility for use in antiperspirants / deodorant applications. INCI NAME: DimethiconeInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc

@Temperature 25.0 °C
0.935 g/cc

@Temperature 77.0 °F
Viscosity Measure 9.5 cSt
9.5 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point 163 °C
325 °F
Open Cup
Optical Properties Metric English Comments
Refractive Index 1.395
1.395