Polymer Property : Flash Point = 213 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 213 °C
415 °F
LG Chemical DINP Plasticizer
Features: LG DINP is used cable and tarpaulin because it can reduce gas generation during operation due to low volatile compared to DOP.Application: Synthetic leather, sheet, power cableInformation ..
Flash Point 213 °C
415 °F
Lubriplate AC-0 Petroleum-Based Air Compressor Fluid
Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar..
Flash Point 213 °C
415 °F
Lubriplate H0-0 Petroleum-Based Heavy-Duty Hydraulic Oil
Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin..
Flash Point 213 °C
415 °F
Lubriplate SPO-222 Petroleum-Based Gear, Bearing, & Recirculating Oil
Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati..
Flash Point 213 °C
415 °F
ASTM D92
ChevronTexaco 100 White Oil
FeaturesChevron Technical White Oils are high quality, highly refined, odorless, tasteless, clear, paraffinic, technical grade white oils.Chevron Technical White Oils are hydrocracked and dewaxed us..
Flash Point 213 °C
415 °F
ASTM D92
ChevronTexaco 100R Neutral Oil
FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o..
Flash Point 213 °C
415 °F
ASTM D92
ChevronTexaco 10-T White Oil
FeaturesChevron White Oils are technical grade oils processed from paraffinic oil. Mixtures of paraffinic and naphthenic hydrocarbons, they are virtually free of nitrogen, sulfur, oxygen, and aroma..
Flash Point 213 °C
415 °F
ChevronTexaco Canopus® 19
Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant ..
Flash Point 213 °C
415 °F
ASTM D92
ChevronTexaco ParaLux® 1001 Paraffinic Process Oil
FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup..
Flash Point 213 °C
415 °F
ASTM D92
ChevronTexaco ParaMount™ 1001 Paraffinic Process Oil
FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur..
Flash Point 213 °C
415 °F
ASTM D92
ChevronTexaco TEGRA® SAE 80W-140 Synthetic Gear Lubricant
FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality, multipurpose gear lubricants.It is manufactured from synthesized hydrocarbon base fluids which have exceptional thermal and oxid..
Flash Point 213 °C
415 °F
ConocoPhillips Hydroclear® 10W-30 Power-D E.O. 10W-30
Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corros..
Flash Point 213 °C
415 °F
ChevronTexaco Capella® WF 100
Texaco Capella WF oils delivers value through:Wax-free — Suitable for ultra-low temperature service.Water-free — Low moisture content prevents icing in refrigeration expansion valves and helps pre..
Flash Point 213 °C
415 °F
PMCC
ACC EP MAP-10 EPI Engineered Polymers Aliphatic Polymer
EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-10 contains 10% NCO. Pa..
Flash Point 213 °C
415 °F
PMCC
ACC EP MAP-14 EPI Engineered Polymers Aliphatic Polymer
EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-14 contains 14% NCO. Pa..
Flash Point 213 °C
415 °F
PMCC
ACC EP MAP-18 EPI Engineered Polymers Aliphatic Polymer
EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-18 contains 18% NCO. Pa..
Flash Point 213 °C
415 °F
PMCC
ACC EP MAP-7.5 EPI Engineered Polymers Aliphatic Polymer
EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-7.5 contains 7.5% NCO. ..
Flash Point 213 °C
415 °F
PMCC
ACC EP MAP-8.5 EPI Engineered Polymers Aliphatic Polymer
EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-8.5 contains 8.5% NCO. ..
Flash Point 213 °C
415 °F
PMCC
ACC EP MAP-Z 14 EPI Engineered Polymers Aliphatic Polymer
EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail..
Flash Point 213 °C
415 °F
PMCC
ACC EP MAP-Z 10 EPI Engineered Polymers Aliphatic Polymer
EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail..
Flash Point 213 °C
415 °F
PMCC
ACC EP MAP-Z 18 EPI Engineered Polymers Aliphatic Polymer
EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail..
Flash Point 213 °C
415 °F
ASTM D-92
ConocoPhillips ANDEROL® SAE 20 White Mineral Oil Food Grade Trolley Oil ISO 46
Description: ANDEROL PQ Trolley Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ Trolley Oil is recomm..