Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 213 °C | 415 °F | |
LG Chemical DINP Plasticizer Features: LG DINP is used cable and tarpaulin because it can reduce gas generation during operation due to low volatile compared to DOP.Application: Synthetic leather, sheet, power cableInformation .. |
|||
Flash Point | 213 °C | 415 °F | |
Lubriplate AC-0 Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Flash Point | 213 °C | 415 °F | |
Lubriplate H0-0 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Flash Point | 213 °C | 415 °F | |
Lubriplate SPO-222 Petroleum-Based Gear, Bearing, & Recirculating Oil Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati.. |
|||
Flash Point | 213 °C | 415 °F | ASTM D92 |
ChevronTexaco 100 White Oil FeaturesChevron Technical White Oils are high quality, highly refined, odorless, tasteless, clear, paraffinic, technical grade white oils.Chevron Technical White Oils are hydrocracked and dewaxed us.. |
|||
Flash Point | 213 °C | 415 °F | ASTM D92 |
ChevronTexaco 100R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Flash Point | 213 °C | 415 °F | ASTM D92 |
ChevronTexaco 10-T White Oil FeaturesChevron White Oils are technical grade oils processed from paraffinic oil. Mixtures of paraffinic and naphthenic hydrocarbons, they are virtually free of nitrogen, sulfur, oxygen, and aroma.. |
|||
Flash Point | 213 °C | 415 °F | |
ChevronTexaco Canopus® 19 Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant .. |
|||
Flash Point | 213 °C | 415 °F | ASTM D92 |
ChevronTexaco ParaLux® 1001 Paraffinic Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
Flash Point | 213 °C | 415 °F | ASTM D92 |
ChevronTexaco ParaMount™ 1001 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Flash Point | 213 °C | 415 °F | ASTM D92 |
ChevronTexaco TEGRA® SAE 80W-140 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality, multipurpose gear lubricants.It is manufactured from synthesized hydrocarbon base fluids which have exceptional thermal and oxid.. |
|||
Flash Point | 213 °C | 415 °F | |
ConocoPhillips Hydroclear® 10W-30 Power-D E.O. 10W-30 Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corros.. |
|||
Flash Point | 213 °C | 415 °F | |
ChevronTexaco Capella® WF 100 Texaco Capella WF oils delivers value through:Wax-free — Suitable for ultra-low temperature service.Water-free — Low moisture content prevents icing in refrigeration expansion valves and helps pre.. |
|||
Flash Point | 213 °C | 415 °F | PMCC |
ACC EP MAP-10 EPI Engineered Polymers Aliphatic Polymer EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-10 contains 10% NCO. Pa.. |
|||
Flash Point | 213 °C | 415 °F | PMCC |
ACC EP MAP-14 EPI Engineered Polymers Aliphatic Polymer EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-14 contains 14% NCO. Pa.. |
|||
Flash Point | 213 °C | 415 °F | PMCC |
ACC EP MAP-18 EPI Engineered Polymers Aliphatic Polymer EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-18 contains 18% NCO. Pa.. |
|||
Flash Point | 213 °C | 415 °F | PMCC |
ACC EP MAP-7.5 EPI Engineered Polymers Aliphatic Polymer EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-7.5 contains 7.5% NCO. .. |
|||
Flash Point | 213 °C | 415 °F | PMCC |
ACC EP MAP-8.5 EPI Engineered Polymers Aliphatic Polymer EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-8.5 contains 8.5% NCO. .. |
|||
Flash Point | 213 °C | 415 °F | PMCC |
ACC EP MAP-Z 14 EPI Engineered Polymers Aliphatic Polymer EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail.. |
|||
Flash Point | 213 °C | 415 °F | PMCC |
ACC EP MAP-Z 10 EPI Engineered Polymers Aliphatic Polymer EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail.. |
|||
Flash Point | 213 °C | 415 °F | PMCC |
ACC EP MAP-Z 18 EPI Engineered Polymers Aliphatic Polymer EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are avail.. |
|||
Flash Point | 213 °C | 415 °F | ASTM D-92 |
ConocoPhillips ANDEROL® SAE 20 White Mineral Oil Food Grade Trolley Oil ISO 46 Description: ANDEROL PQ Trolley Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ Trolley Oil is recomm.. |