Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Boiling Point 252 °C

@Pressure 600000 MPa
486 °F

@Pressure 8.70e+7 psi
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..