Thermal Properties Metric English Comments
Boiling Point 343 °C
649 °F
atmospheric boiling point, 10% fraction; ASTM D1160
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
Description: Paratherm NF® heat transfer fluid is highly efficient, thermally stable and cost-effective. It is also non-fouling, low pour and odor free. Completely non-toxic, it is exceptionally ..