Material Notes:
Description: Paratherm NF® heat transfer fluid is highly efficient, thermally stable and cost-effective. It is also non-fouling, low pour and odor free. Completely non-toxic, it is exceptionally safe to use and easy to dispose. Used fluid can be safely combined with spent lubricating oils and recycled locally (EPA, citation 57FR21524). Information provided by Paratherm Corporation.
Physical Properties Metric English Comments
Density 0.869 g/cc

@Temperature 23.9 °C
0.0314 lb/in³

@Temperature 75.0 °F
Solubility 10 ppm
10 ppm
H<sub>2</sub>, by weight, at 760 mm Hg/25°C
Molecular Weight 350 g/mol
350 g/mol
average; ASTM D2502
Vapor Pressure 0.00003447 bar

@Temperature 93.3 °C
0.02586 torr

@Temperature 200 °F
0.0002068 bar

@Temperature 149 °C
0.1551 torr

@Temperature 300 °F
0.0101 bar

@Temperature 204 °C
7.60 torr

@Temperature 400 °F
0.0667 bar

@Temperature 260 °C
50.0 torr

@Temperature 500 °F
0.325 bar

@Temperature 316 °C
244 torr

@Temperature 600 °F
Surface Tension 29.6 dynes/cm
29.6 dynes/cm
at 760 mm Hg/20°C
Thermal Properties Metric English Comments
Heat of Vaporization 211 J/g
90.7 BTU/lb
calculated
CTE, linear 547 µm/m-°C

@Temperature 20.0 °C
304 µin/in-°F

@Temperature 68.0 °F
Boiling Point 343 °C
649 °F
atmospheric boiling point, 10% fraction; ASTM D1160
Maximum Service Temperature, Air 316 °C
600 °F
optimum use range
<= 338 °C
<= 640 °F
max. recommended film temperature
Minimum Service Temperature, Air 48.9 °C
120 °F
optimum use range
Pour Point -42.8 °C
-45.0 °F
ASTM D97
Flash Point 168 °C
335 °F
pmcc; ASTM D93
174 °C
345 °F
coc; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4768

@Temperature 20.0 °C
1.4768

@Temperature 68.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
DC; ASTM D1169
Dielectric Constant 2.17

@Frequency 1e+6 Hz
2.17

@Frequency 1e+6 Hz
Dielectric Strength 3.00 - 4.00 kV/mm

@Temperature 20.0 °C
76.2 - 102 kV/in

@Temperature 68.0 °F
ASTM D877
Dissipation Factor 0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
Descriptive Properties Value Comments
Appearance transparent, colorless
Autoignition 690°F
ASTM D2155
691°F
ASTM E659-78
Feedstock NF/USP hydrotreated hydrocarbon
Fire point 386°F
ASTM D92, coc
Odor none
Pumpability -13°F
centrifugal at 2000 centipoise