Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 326 °C | 619 °F | |
BASF Dicykan 4,4'-Diaminodicyclohexylmethane Formula: C17H30N2CAS: 1761-71-3Description: Dicykan is a colorless to yellow solidified mass, with an amine-like odor. It is soluble in organic solvents.Synonyms: DC, DicykaneApplications: Intermedi.. |