Material Notes:
Formula: C17H30N2CAS: 1761-71-3Description: Dicykan is a colorless to yellow solidified mass, with an amine-like odor. It is soluble in organic solvents.Synonyms: DC, DicykaneApplications: Intermediate used in Hardeners for epoxy resins and Initial product for chemical synthesesInformation provided by BASF
Physical Properties Metric English Comments
Molecular Weight 74.1 g/mol
74.1 g/mol
Thermal Properties Metric English Comments
Melting Point 33.5 - 44.0 °C
92.3 - 111 °F
Boiling Point 326 °C
619 °F
Flash Point 159 °C
318 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99%
Ignition Temperature 305°C