Thermal Properties Metric English Comments
Boiling Point 1196 °C
2185 °F
American Elements Ytterbium Nanoparticles
General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec..