Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 1196 °C | 2185 °F | |
American Elements Ytterbium Nanoparticles General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec.. |