Thermal Properties Metric English Comments
Softening Point 883 °C
1620 °F
10<sup>7.6</sup> dPa-s
Schott AF 45 Thin Borosilicate Glass
AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc..