Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 883 °C | 1620 °F | 10<sup>7.6</sup> dPa-s |
Schott AF 45 Thin Borosilicate Glass AF 45 is an alkali-free modified borosilicate glass with a high content of BaO and Al2O3. AF 45 with, its specific properties and large range of different thicknesses with tight tolerances, is exc.. |