Thermal Properties Metric English Comments
Softening Point 712 °C
1310 °F
Schott S8807 Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
Softening Point 712 °C
1310 °F
Corning 7052 Alkali Barium Borosilicate Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated.