Schott S8807 Contrast Enhancement Filter

Category Ceramic , Glass , Filter
Manufacturer Schott North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott S8807 Contrast Enhancement Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 2.91 g/cc
0.105 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.90 µm/m-°C

@Temperature 20.0 - 300 °C
4.94 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 570 °C
1060 °F
Softening Point 712 °C
1310 °F
Working Point 934 °C
1710 °F
Annealing Point 576 °C
1070 °F
Strain Point 555 °C
1030 °F
Optical Properties Metric English Comments
Refractive Index 1.563
1.563
n<sub>d</sub>, Mercury
Transmission, Visible 72.5 %

@Wavelength 544 nm
72.5 %

@Wavelength 544 nm
78.5 %

@Wavelength 618 nm
78.5 %

@Wavelength 618 nm
79 %

@Wavelength 445 nm
79 %

@Wavelength 445 nm
Descriptive Properties Value Comments
Color Violet