Thermal Properties Metric English Comments
Softening Point 59.0 - 63.0 °C
138 - 145 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 108 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® 108 is a linear, aromatic polycaprolactone-based polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a medium thermoplasti..
Softening Point 59.0 - 71.0 °C
138 - 160 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-661 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..