Polymer Property : Softening Point = 145 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 59.0 - 63.0 °C
138 - 145 °F
MQSA 70 A
Lubrizol Advanced Materials PEARLBOND® 108 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® 108 is a linear, aromatic polycaprolactone-based polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a medium thermoplasti..