Thermal Properties Metric English Comments
Softening Point 480 °C
896 °F
Ferro EG 4020 Display Device
Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas..
Softening Point 480 °C
896 °F
Permanent Softening
CMW® 328 Copper Alloy
CMW® 328 material is a high strength, high conductivity copper base alloy. CMW® 328 is heat treatable. Optimum mechanical and physical properties of CMW® 328 material are developed by heat treatm..