Ferro EG 4020 Display Device

Category Ceramic , Glass
Manufacturer Ferro Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ferro EG 4020 Display Device.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and passivation of soda lime glass packages, including plasma display panels and tubes.Information provided by Ferro Corporation
Physical Properties Metric English Comments
Density 5.08 g/cc
0.184 lb/in³
Particle Size >= 16 µm
>= 16 µm
50% of particles
<= 105 µm
<= 105 µm
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C
4.61 µin/in-°F
at Set Pt.
7.75 µm/m-°C

@Temperature 260 °C
4.31 µin/in-°F

@Temperature 500 °F
Softening Point 480 °C
896 °F
Transformation Temperature 410 °C
770 °F
Processing Properties Metric English Comments
Processing Temperature 600 °C
1110 °F
Typical Firing Temperature; Typical Firing Time: 10 min.