Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 129.5 °C | 265.1 °F | ETM 22-24 |
ExxonMobil ESCOREZ™ 5637 Petroleum Hydrocarbon Resin Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and metallocene polyolefines. Avail.. |