ExxonMobil ESCOREZ™ 5637 Petroleum Hydrocarbon Resin

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Adhesive
Manufacturer Exxon Chemical
Trade Name Escorez™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil ESCOREZ™ 5637 Petroleum Hydrocarbon Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and metallocene polyolefines. Availability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Viscosity 1450 cP

@Temperature 180 °C
1450 cP

@Temperature 356 °F
Melt; ETM 22-31
Molecular Weight 570 g/mol
570 g/mol
Mn; ETM 300-83
820 g/mol
820 g/mol
Mw; ETM 300-83
Thermal Properties Metric English Comments
Softening Point 129.5 °C
265.1 °F
ETM 22-24
Glass Transition Temp, Tg 80.0 °C
176 °F
ETM 300-90
Descriptive Properties Value Comments
Aromacity, % 6