Polymer Property : Softening Point = 1870 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 1020 °C
1870 °F
3M W-210 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..
Softening Point 1020 °C
1870 °F
3M W-410 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..
Softening Point 1020 °C
1870 °F
3M W-610 Ceramic Microspheres
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l..