Thermal Properties Metric English Comments
Softening Point 925 °C
1700 °F
Ferro EG 2705 Glaze and Sealant Glass
Glass Type: Ca-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulat..
Softening Point 926 °C
1700 °F
Corning 1724 Aluminosilicate Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated.