Thermal Properties Metric English Comments
Softening Point 775 °C
1430 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8487 Borosilicate Glass
Borosilicate glass for sealing to tungsten Backlights, flash lamps, lamp bulbs, exhaust and flare bulbs The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is ..
Softening Point 775 °C
1430 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Schott Glass 8687 Borosilicate Glass
Borosilicate glass for sealing to tungsten, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi..
Softening Point 775 °C
1430 °F
Zircar Refractory Composites RS-DD Refractory Sheet
ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She..