Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Softening Point = 130 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point 110 - 130 °C
230 - 266 °F
MQSA 70 A
Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane
Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softe..
Softening Point 110 - 130 °C
230 - 266 °F
MQSA 70 A
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane
Pearlbondâ„¢ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus..
Softening Point 110 - 130 °C
230 - 266 °F
MQSA 70A
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft..
Softening Point 110 - 130 °C
230 - 266 °F
flow beginning
Taiwan Sheen Soon Sheenthane® AH-706L TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hotmelt adhesiveHydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. U..
Softening Point 110 - 130 °C
230 - 266 °F
Suqian Unitechem Light Stabilizer 944
Chemical Name: Poly-{[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidyl)imino]-1,6-hexanediyl[(2,2,6,6-tetramethyl-4-piperidyl)imino]}CAS NO.: 70624-18-9M..
Copyright © lookpolymers.com All Rights Reserved