Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlbond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlbondâ„¢ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softening point.Application: Pearlbondâ„¢ 125H can be used for making heat-sealable fabrics (thermobonding), obtained by coating processes such as scattering or dot-coating (powder or paste). In all cases, the product is previously ground into powder, by cryogenic grinding. The particle size of the powder will depend on the application technique to be used.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Viscosity 890000 cP

@Temperature 160 °C
890000 cP

@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Melt Flow 35 - 55 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 - 55 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ISO 868
Tensile Strength at Break 18.0 MPa
2610 psi
ISO 527
Elongation at Break 520 %
520 %
ISO 527
100% Modulus 0.00400 GPa
0.580 ksi
ISO 527
300% Modulus 0.00700 GPa
1.02 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 130 - 140 °C
266 - 284 °F
MQSA 111
Softening Point 110 - 130 °C
230 - 266 °F
MQSA 70A
Processing Properties Metric English Comments
Zone 1 120 - 130 °C
248 - 266 °F
Zone 2 130 - 140 °C
266 - 284 °F
Zone 3 140 - 150 °C
284 - 302 °F
Zone 4 145 - 155 °C
293 - 311 °F
Die Temperature 145 - 155 °C
293 - 311 °F