Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 25.0 - 174 °C | 77.0 - 345 °F | Average value: 71.4 °C Grade Count:236 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 25.0 °C | 77.0 °F | ASTM D648 |
Clariant Renol PPT20BN-346 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |