Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 25.0 - 174 °C
77.0 - 345 °F
Average value: 71.4 °C Grade Count:236
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Deflection Temperature at 1.8 MPa (264 psi) 163 - 174 °C
325 - 345 °F
Average value: 169 °C Grade Count:6
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..