Deflection Temperature at 1.8 MPa (264 psi) 73.00 °C
163.4 °F
unannealed; ASTM D-648
Axiall Suprel® SVA 9301 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li..