Axiall Suprel® SVA 9301 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name Suprel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall Suprel® SVA 9301 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability listings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.4 MPa
6300 psi
ASTM D-638
Tensile Modulus 2.61 GPa
379 ksi
ASTM D-638
Flexural Strength 62.7 MPa
9100 psi
ASTM D-790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D-790
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
0.500 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D-256
4.59 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
8.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
unannealed; ASTM D-648
84.00 °C
183.2 °F
annealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 73.00 °C
163.4 °F
unannealed; ASTM D-648
80.0 °C
176 °F
annealed; ASTM D-648
Vicat Softening Point 94.4 °C
202 °F
annealed; ASTM D-1525A
UL RTI, Electrical 50.0 °C
122 °F
UL-746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
5VA

@Thickness 2.53 mm
5VA

@Thickness 0.0996 in