Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648 |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648 |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648 |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648 |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648 |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648 |
Spartech EP6220 Filled and Reinforced Copolymer Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648 |
Spartech PP7110 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE TM20 20% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE TM20 UV BK 20% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: BlackInformation provided by TP Composi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HDPE TM25 25% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 25% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648 |
Westlake Plastics Lennite® SD-P UHMW-PE (static dissipative) Carbon-powder filled, self-lubricating, moisture-repellent material with resistivity levels in the 10^5-10^9 range. This material has the highest impact strength, is lightweight, has excellent abra.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648B |
ExxonMobil HDPE HD 6706.17 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ASTM D648B |
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | ISO 75-2/A |
ExxonMobil PP8013L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 46.1 °C | 115 °F | |
Aclo Accutech Polypropylene Copolymer CP0437C10L1 Calcium Reinforced |