Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | ASTM D648 |
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1240MGHL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement -15% Filler by Weight, Mineral -25% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat S.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | ASTM D648 |
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M36 HS BK 36% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 36% Filler by Weight and Mineral Filler, 36% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 HS L NAT 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 IG BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF/M40 L BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PET GF55 X 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 GF30 FR HS2 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 229 °C | 445 °F | ASTM D648 |
Solvay Specialty Polymers Xydar® M-345 Liquid Crystal Polymer, 45% Mineral Filled
(discontinued **) XYDAR M-345 Liquid Crystal Polymer (LCP) is a 45% mineral-filled injection molding grade with exceptional moldability. XYDAR M-345 resin can fill very thin walls over long flow lengths with little o.. |