Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 169.4 °C
336.9 °F
ASTM D648
CRP Technology Windform® GT Polyamide Glass Composite
Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter...