Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 169.4 °C | 336.9 °F | ASTM D648 |
CRP Technology Windform® GT Polyamide Glass Composite Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter... |