Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 325 °C | 617 °F | ISO 75-f |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 325 °C @Thickness 3.20 mm |
617 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 325 °C | 617 °F | DIN 53 461 |
Ensinger TECASINT™ 2011 Polyimide (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 325 °C | 617 °F | ISO 75-f |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |