Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 315 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 240 - 315 °C
464 - 599 °F
Average value: 286 °C Grade Count:14
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Deflection Temperature at 1.8 MPa (264 psi) 164 - 315 °C
327 - 599 °F
Average value: 238 °C Grade Count:61
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..