Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 177 - 259 °C
350 - 498 °F
Average value: 239 °C Grade Count:33
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Deflection Temperature at 1.8 MPa (264 psi) 230 - 259 °C
446 - 498 °F
Average value: 248 °C Grade Count:28
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..