Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 235.00 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 112.78 °C
235.00 °F
ASTM D648
Lucent Polymers GPP-110 Polypropylene Homopolymer, 10% Glass Fiber Reinforced, Chemically Coupled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 112.78 °C
235.00 °F
ASTM D648
Lucent Polymers PC/ABS-1020 Polycarbonate+ABS, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.