Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 112.78 °C | 235.00 °F | ASTM D648 |
Lucent Polymers GPP-110 Polypropylene Homopolymer, 10% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 112.78 °C | 235.00 °F | ASTM D648 |
Lucent Polymers PC/ABS-1020 Polycarbonate+ABS, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |