Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | ASTM D-648 |
Plaskolite Optix® CA - 71 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | ASTM D-648 |
Plaskolite Optix® CP - 71 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | ASTM D-648 |
Plaskolite Optix® CP - 71 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | ASTM D-648 |
Plaskolite West Optix® CP - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | ASTM D-648 |
Plaskolite West Optix® CP - 71 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers SAN 300 Natural Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS CR X Availability: North AmericaForms: PelletsFeatures: Good Chemical ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS CR X BK Availability: North AmericaForms: PelletsFeatures: Good Chemical ResistanceUses: Electrical PartsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 96.7 °C | 206 °F | ASTM D-648 |
Plaskolite West Optix® CA - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |