Techmer ES Plastiblend® ABS CR X

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Techmer ES
Trade Name Plastiblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plastiblend® ABS CR X.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Good Chemical ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength at Break 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Flexural Yield Strength 64.8 MPa
9400 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 2.40 J/cm

@Thickness 3.17 mm
4.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.7 °C
206 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: