Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 87.0 - 91.0 °C @Thickness 3.20 mm |
189 - 196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP COLORCOMP NX05467 PC+ABS LNP* COLORCOMP* NX05467 is an unfilled Polycarbont+ABS resin. Added features of this grade are: Non-Chlorinated, Non-Brominated Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.0 - 91.0 °C | 140 - 196 °F | Average value: 79.4 °C Grade Count:71 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |