Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP COLORCOMP NX05467 PC+ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP NX05467 PC+ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* COLORCOMP* NX05467 is an unfilled Polycarbont+ABS resin. Added features of this grade are: Non-Chlorinated, Non-Brominated Flame Retardant.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 66.0 MPa
9570 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 2.68 GPa
389 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.0 - 91.0 °C

@Thickness 3.20 mm
189 - 196 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 0.700 mm
HB

@Thickness 0.0276 in
UL 94
V-1

@Thickness 1.20 mm
V-1

@Thickness 0.0472 in
UL 94
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
5VB

@Thickness 2.10 mm
5VB

@Thickness 0.0827 in
UL 94
5VA

@Thickness 3.40 mm
5VA

@Thickness 0.134 in
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Dielectric Constant 2.7

@Frequency 1.00e+6 Hz
2.7

@Frequency 1.00e+6 Hz
IEC 60250
2.8

@Frequency 60.0 Hz
2.8

@Frequency 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm

@Thickness 3.20 mm
432 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
25.6 kV/mm

@Thickness 1.60 mm
650 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
37.6 kV/mm

@Thickness 0.800 mm
955 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor 0.0040

@Frequency 50.0 - 60.0 Hz
0.0040

@Frequency 50.0 - 60.0 Hz
IEC 60250
0.0080

@Frequency 1.00e+6 Hz
0.0080

@Frequency 1.00e+6 Hz
IEC 60250