Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 89.4 °C

@Thickness 6.40 mm
193 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact
Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
Deflection Temperature at 1.8 MPa (264 psi) 89.4 °C
193 °F
ASTM D648
Spartech CastAlloy Weatherable Sheet
Description: Weatherable SheetInformation provided by Spartech.
Deflection Temperature at 1.8 MPa (264 psi) 89.4 °C
193 °F
ASTM D648
Americas Styrenics STYRON® 686E High Heat Crystal Polystyrene
Product CharacteristicsExceptional balance between heat resistance, toughness and flowGood dimensional stability and excellent clarityFood Contact CompliantTypical ApplicationsFoamed PS sheets used ..