Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 179 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.3 - 179 °C
200 - 354 °F
Average value: 144 °C Grade Count:10
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..
Deflection Temperature at 1.8 MPa (264 psi) 132 - 179 °C
270 - 354 °F
Average value: 153 °C Grade Count:32
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..