Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 74.4 °C @Thickness 3.18 mm |
166 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 87150 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 74.3 °C | 166 °F | Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion LR610 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 74.4 °C | 166 °F | annealed; ASTM D648 |
Kleerdex Kydex® P90 Acrylic/PVC Extrusion Compound
(discontinued **) Low heat release aviation gradeApplications: Kydex P90 is designed for extrusion of profiles which need to meet the highest flammability requirement of PAR 25.853a for vertical burn, rate of heat re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 74.5 °C @Thickness 3.18 mm |
166 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |