Kleerdex Kydex® P90 Acrylic/PVC Extrusion Compound  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® P90 Acrylic/PVC Extrusion Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low heat release aviation gradeApplications: Kydex P90 is designed for extrusion of profiles which need to meet the highest flammability requirement of PAR 25.853a for vertical burn, rate of heat release, and smoke generation.Features: Kydex IM90 is available in many standard and custom colors enabling you to satisfy both the functional and aesthetic requirements of any aircraft interior. Kydex IM90 is very resistant to a wide range of concentrated chemicals, and is therefore easy to clean with aggressive cleaners. Ammoniated cleaners should be avoided since they can leave a residue. Most importantly, Kydex IM90 meets the stringent requirements for the FAR 25.853 paragraph (d) in all thicknesses and colors.Processing: This compound should be processed using rigid PVC extrusion equipment under standard PVC operating conditions. Barrel temperatures in an extruder should be set at 166-171°C and adapter and die temperatures should be 171-177°C. Screw RPMs of 23 to 33 are typical. Typically single screw extruders are used for pelletized material and conical twin screw extruders for powder. Unlike other thermoplastic resins, pre-drying is not required.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 195 %
195 %
ASTM D638
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 2.989 GPa
433.5 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 74.4 °C
166 °F
annealed; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 160 - 182 °C
320 - 360 °F
Barrel Temp
Middle Barrel Temperature 160 - 182 °C
320 - 360 °F
Adapter Temperature 171 - 177 °C
340 - 350 °F
Die Temperature 171 - 177 °C
340 - 350 °F
Dry Time 0.0 hour
0.0 hour
Drying typically not required