Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 71.0 - 145 °C | 160 - 293 °F | Average value: 102 °C Grade Count:14 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 125 - 145 °C | 257 - 293 °F | Average value: 135 °C Grade Count:9 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 106 - 145 °C | 223 - 293 °F | Average value: 128 °C Grade Count:17 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |