Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 61.22 °C | 142.2 °F | ASTM D-648 |
Axiall 9190 Rigid PVC, Molding Georgia Gulf 9190 was developed to aid compliance with source reduction initiatives especially when low temperature impact strength is a concern. It has superior properties, which in most cases wil.. |