Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 60.6 °C @Thickness 3.18 mm |
141 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 87358 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.6 °C | 141 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/6,6 IM HS L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.4 °C | 141 °F | ISO 75-2 |
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 60.6 °C | 141 °F | ASTM D648 |
Westlake Plastics Pomalux® SD-A Acetal Copolymer (anti-static) Non-carbon-filled, permanently static-dissipative material which is non-migratory and non-humidity dependent. With enhanced lubricity, POMALUX SD-A provides superior wear resistance and ease of mac.. |